Causes Of Lamination In Steel

Can cause a poor weld to be made.
Causes of lamination in steel. Also surface coatings such as paints and films can delaminate from the coated substrate. Electrical steel is usually manufactured in cold rolled strips less than 2 mm thick. Lamination means a process applied to alloys metal plastics and other materials consistent in subjecting the material to the constriction action by a machine called a rolling mill made up of two conjugated cylinders fig 1 rotating in the opposite direction with the same peripheral speed so that the material is forced to assume a section corresponding to the free light that remains among the cylinders themselves. The wrong temperature impurities etc.
Processing can create layers in materials such as steel formed by rolling and plastics and metals from 3d printing which can fail from layer separation. Laminations may be cut to their finished shape by a punch and die. The laminate will stick together but applying and bending force can cause it to delaminate. These strips are cut to shape to make laminations which are stacked together to form the laminated cores of transformers and the stator and rotor of electric motors.
Electrical steel is an iron alloy tailored to produce specific magnetic properties. These folds and layers do not bond together and will separate when metal is worked. Plate lamination in carbon steel happens when folds or layers of plates are rolled together into a single plate thickness. Rolled steel bar stock is made by rolling and rerolling steel billets until the desired shape and dimensions are attained.
A variety of materials including laminate composites and concrete can fail by delamination.